Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Abrasion resistance | 40 mm³ Show Supplier Material materials with Abrasion resistance of 40 mm³ | dry | ISO 4649 |
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | Sim. to ISO 62 | |
Wasserabsorption | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. |
Druckverformungsrest | 37 [-] Show Supplier Material materials with Druckverformungsrest of 37 [-] | ISO 815 | for 24h | |
Elastizitätsmodul | 0.081 GPa Show Supplier Material materials with Elastizitätsmodul of 0.081 GPa | cond. | ISO 527-1/-2 | |
0.088 GPa Show Supplier Material materials with Elastizitätsmodul of 0.088 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore A | 92 [-] Show Supplier Material materials with Härte, Shore A of 92 [-] | ISO 7619-1 | for 3 seconds | |
Härte, Shore D | 41 [-] Show Supplier Material materials with Härte, Shore D of 41 [-] | dry | ISO 7619-1 | 15 seconds |
Reißfestigkeit | 77 kN/m Show Supplier Material materials with Reißfestigkeit of 77 kN/m | ISO 34-1 | ||
Schlagfestigkeit, Charpy gekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | |
Streckgrenze | 13 MPa Show Supplier Material materials with Streckgrenze of 13 MPa | cond. | ISO 527-1/-2 | |
14 MPa Show Supplier Material materials with Streckgrenze of 14 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.0002 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0002 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 147 °C Show Supplier Material materials with Schmelzpunkt of 147 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 111 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 111 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 6 [-] | dry | 1MHz | IEC 60250 |
9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 9 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 43 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 43 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 3e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 3e+12 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.112 [-] Show Supplier Material materials with Verlustfaktor of 0.112 [-] | dry | 1MHz | IEC 60250 |
0.209 [-] Show Supplier Material materials with Verlustfaktor of 0.209 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 1.6e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1.6e+13 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 0.83 g/cm³ Show Supplier Material materials with Density of melt of 0.83 g/cm³ | |||
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | dry | ISO 294-4 | |
1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | dry | ISO 294-4 | Transverse | |
Specific heat capacity melt | 2500 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2500 J/(kg·K) | |||
Thermal conductivity of melt | 0.18 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.18 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Conveyor Belts and Pulleys,Nylon Film Modification,Footwear - Outsoles,Ski Boots | |
Processing methods | Injection Molding: Extrusion: |