Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.6 % Show Supplier Material materials with Moisture absorption of 0.6 % | Sim. to ISO 62 | |
Wasserabsorption | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal |
Elastizitätsmodul | 0.165 GPa Show Supplier Material materials with Elastizitätsmodul of 0.165 GPa | cond. | ISO 527-1/-2 | |
0.17 GPa Show Supplier Material materials with Elastizitätsmodul of 0.17 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 25 % Show Supplier Material materials with Elongation at yield of 25 % | cond., dry | ISO 527-1/-2 | |
Härte, Shore D | 50 [-] Show Supplier Material materials with Härte, Shore D of 50 [-] | dry | ISO 7619-1 | 15 seconds |
Schlagfestigkeit, Charpy gekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | |
Streckgrenze | 12 MPa Show Supplier Material materials with Streckgrenze of 12 MPa | cond. | ISO 527-1/-2 | |
18 MPa Show Supplier Material materials with Streckgrenze of 18 MPa | dry | ISO 527-1/-2 |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Conveyor Belts and Pulleys | |
Certifications | Food Contact | |
Processing methods | Injection Molding: Extrusion: |