Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.09 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 | |
Wasserabsorption | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal |
Elastizitätsmodul | 0.298 GPa Show Supplier Material materials with Elastizitätsmodul of 0.298 GPa | cond. | ISO 527-1/-2 | |
0.305 GPa Show Supplier Material materials with Elastizitätsmodul of 0.305 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 31 % Show Supplier Material materials with Elongation at yield of 31 % | dry | ISO 527-1/-2 | |
36 % Show Supplier Material materials with Elongation at yield of 36 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 60 [-] Show Supplier Material materials with Härte, Shore D of 60 [-] | dry | ISO 7619-1 | 15 seconds |
Schlagfestigkeit, Charpy gekerbt | No Break at 23°C | cond. | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | |
Streckgrenze | 12 MPa Show Supplier Material materials with Streckgrenze of 12 MPa | cond. | ISO 527-1/-2 | |
19 MPa Show Supplier Material materials with Streckgrenze of 19 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00022 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00022 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 159 °C Show Supplier Material materials with Schmelzpunkt of 159 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 5500 Ω/sq Show Supplier Material materials with Surface resistivity of 5500 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1.1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1.1e+07 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 5 cm³/10min | dry | ISO 1133 | 250°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Alternative Fuel Systems - CNG, LPG, LNG Lines and Tanks,Underground Fuel Containment | |
Fillers | Carbon Black | |
Processing methods | Injection Molding: Extrusion: |