Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Abrasion resistance | 55 mm³ Show Supplier Material materials with Abrasion resistance of 55 mm³ | dry | ISO 4649 |
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | Sim. to ISO 62 | |
Sauerstoffindex | 20 % Show Supplier Material materials with Sauerstoffindex of 20 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 1.1 % Show Supplier Material materials with Wasserabsorption of 1.1 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal |
Druckverformungsrest | 47 [-] Show Supplier Material materials with Druckverformungsrest of 47 [-] | ISO 815 | for 24h | |
Elastizitätsmodul | 0.285 GPa Show Supplier Material materials with Elastizitätsmodul of 0.285 GPa | cond. | ISO 527-1/-2 | |
0.307 GPa Show Supplier Material materials with Elastizitätsmodul of 0.307 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 22 % Show Supplier Material materials with Elongation at yield of 22 % | cond., dry | ISO 527-1/-2 | |
Härte, Shore D | 58 [-] Show Supplier Material materials with Härte, Shore D of 58 [-] | dry | ISO 7619-1 | 15 seconds |
Reißfestigkeit | 127 kN/m Show Supplier Material materials with Reißfestigkeit of 127 kN/m | ISO 34-1 | ||
Schlagfestigkeit, Charpy gekerbt | No Break at 23°C | cond., dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU | |
Streckgrenze | 22 MPa Show Supplier Material materials with Streckgrenze of 22 MPa | cond. | ISO 527-1/-2 | |
23 MPa Show Supplier Material materials with Streckgrenze of 23 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00014 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00014 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 169 °C Show Supplier Material materials with Schmelzpunkt of 169 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 157 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 157 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB and yellow card available |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 1MHz | IEC 60250 |
9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 9 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 42.5 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 42.5 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.0757 [-] Show Supplier Material materials with Verlustfaktor of 0.0757 [-] | dry | 1MHz | IEC 60250 |
0.144 [-] Show Supplier Material materials with Verlustfaktor of 0.144 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 9e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 9e+13 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 0.83 g/cm³ Show Supplier Material materials with Density of melt of 0.83 g/cm³ | |||
Schrumpfung | 1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | dry | ISO 294-4 | |
1.4 % Show Supplier Material materials with Schrumpfung of 1.4 % | dry | ISO 294-4 | Transverse | |
Specific heat capacity melt | 2800 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2800 J/(kg·K) | |||
Thermal conductivity of melt | 0.18 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.18 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Conveyor Belts and Pulleys,Pneumatic Tubing,Tubing and Hoses,Hook and Loop Fasteners,Footwear - Outsoles,Ski Boots,Sports Equipment | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: Extrusion: |