Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | Sim. to ISO 62 | |
Wasserabsorption | 1.1 % Show Supplier Material materials with Wasserabsorption of 1.1 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.39 GPa Show Supplier Material materials with Elastizitätsmodul of 0.39 GPa | cond. | ISO 527-1/-2 | ||
0.414 GPa Show Supplier Material materials with Elastizitätsmodul of 0.414 GPa | dry | ISO 527-1/-2 | |||
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | cond. | ISO 527-1/-2 | ||
22 % Show Supplier Material materials with Elongation at yield of 22 % | dry | ISO 527-1/-2 | |||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 7619-1 | 15 seconds | |
Reißfestigkeit | 149 kN/m Show Supplier Material materials with Reißfestigkeit of 149 kN/m | ISO 34-1 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 120 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 120 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU | ||
Streckgrenze | 26 MPa Show Supplier Material materials with Streckgrenze of 26 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00016 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00016 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 172 °C Show Supplier Material materials with Schmelzpunkt of 172 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 164 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 164 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB, At Thickness 3.1 mm IEC 60695-11-10: HB and yellow card available |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 |
Surface resistivity | 4e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 4e+13 Ω/sq | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 0.83 g/cm³ Show Supplier Material materials with Density of melt of 0.83 g/cm³ | |||
Schrumpfung | 1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | dry | ISO 294-4 | |
1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | ISO 294-4 | Transverse | |
Specific heat capacity melt | 2700 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2700 J/(kg·K) | |||
Thermal conductivity of melt | 0.2 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.2 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Textile - Others,Footwear - Outsoles,Ski Boots,Sports Equipment | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: Extrusion: |