Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | Sim. to ISO 62 | |
Wasserabsorption | 0.9 % Show Supplier Material materials with Wasserabsorption of 0.9 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.51 GPa Show Supplier Material materials with Elastizitätsmodul of 0.51 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 18 % Show Supplier Material materials with Elongation at yield of 18 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 26 MPa Show Supplier Material materials with Streckgrenze of 26 MPa | cond. | ISO 527-1/-2 |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Nylon Film Modification,Healthcare-Other,IV Bags,Medical Catheters | |
Certifications | USP Class VI | |