Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | Sim. to ISO 62 | |
Wasserabsorption | 0.9 % Show Supplier Material materials with Wasserabsorption of 0.9 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.51 GPa Show Supplier Material materials with Elastizitätsmodul of 0.51 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 18 % Show Supplier Material materials with Elongation at yield of 18 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 7619-1 | 15 seconds | |
Reißfestigkeit | 166 kN/m Show Supplier Material materials with Reißfestigkeit of 166 kN/m | ISO 34-1 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00012 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00012 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 174 °C Show Supplier Material materials with Schmelzpunkt of 174 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 164 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 164 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 1MHz | IEC 60250 |
7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 44.5 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 44.5 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 1.84e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1.84e+14 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.0586 [-] Show Supplier Material materials with Verlustfaktor of 0.0586 [-] | dry | 1MHz | IEC 60250 |
0.163 [-] Show Supplier Material materials with Verlustfaktor of 0.163 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 8e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 8e+13 Ω·cm | dry | IEC 60093 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Hook and Loop Fasteners,Textile - Others,Footwear - Outsoles | |
Processing methods | Injection Molding: Extrusion: |