Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1 % Show Supplier Material materials with Moisture absorption of 1 % | Sim. to ISO 62 | |
Wasserabsorption | 28 % Show Supplier Material materials with Wasserabsorption of 28 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. |
Elastizitätsmodul | 0.045 GPa Show Supplier Material materials with Elastizitätsmodul of 0.045 GPa | cond. | ISO 527-1/-2 | |
Härte, Shore D | 35 [-] Show Supplier Material materials with Härte, Shore D of 35 [-] | dry | ISO 7619-1 | 15 seconds |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 158 °C Show Supplier Material materials with Schmelzpunkt of 158 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Breathable Films - Housewrap,Hot Melt Adhesives - Sports Apparel and Underwear | |
Processing methods | Extrusion: |