Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 28 % Show Supplier Material materials with Bio-based content of 28 % | ||
32 % Show Supplier Material materials with Bio-based content of 32 % | |||
Dichte | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 | |
Wasserabsorption | 1.3 % Show Supplier Material materials with Wasserabsorption of 1.3 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. |
Elastizitätsmodul | 0.04 GPa Show Supplier Material materials with Elastizitätsmodul of 0.04 GPa | cond. | ISO 527-1/-2 | |
Härte, Shore D | 25 [-] Show Supplier Material materials with Härte, Shore D of 25 [-] | dry | ISO 7619-1 | 15 seconds |
Schlagfestigkeit, Charpy gekerbt | No Break at 23 and -30°C | cond., dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Breathable Films - Housewrap,Permanent Antistatic Solutions,Eyewear Frames,Footwear - Midsoles / Foam | |
Processing methods | Injection Molding: Extrusion: |