Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 93 % Show Supplier Material materials with Bio-based content of 93 % | ||
97 % Show Supplier Material materials with Bio-based content of 97 % | |||
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.8 % Show Supplier Material materials with Moisture absorption of 0.8 % | Sim. to ISO 62 | |
Wasserabsorption | 0.7 % Show Supplier Material materials with Wasserabsorption of 0.7 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.56 GPa Show Supplier Material materials with Elastizitätsmodul of 0.56 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 28 % Show Supplier Material materials with Elongation at yield of 28 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 65 [-] Show Supplier Material materials with Härte, Shore D of 65 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 33 MPa Show Supplier Material materials with Streckgrenze of 33 MPa | cond. | ISO 527-1/-2 |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Eyewear Frames,Footwear - Outsoles,Ski Boots | |
Processing methods | Injection Molding: Extrusion: |