Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | dry | ISO 1183 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 115 °C Show Supplier Material materials with Schmelzpunkt of 115 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 10 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 10 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior,Hot Melt Adhesives - Sports Apparel and Underwear,Textile - Others |