Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Platamid® H 2513 Powder
Copolyamide Hot Melt Adhesive / Textile Applications
Platamid® H 2513 Powder is a medium melt viscosity copolyamide adhesive powder for the production of fusible interlinings.
Platamid® H 2513 Powder offers an excellent laundry resistance up to 60°C and an excellent resistance to all kind of steam treatment.
This product is available in different grain sizes:
PACKAGING
Platamid® H 2513 PTA 170 is delivered in 20 kg sealed bags and 500 kg sealed big bags (GRVS). Platamid® H 2513 PA 80 and Platamid ® H 2513 PTA 170/20 are delivered in 20 kg sealed bags.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Diese Materialdaten wurden von Arkema Technical Polymers zur Verfügung gestellt
All categories
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 128 °C Show Supplier Material materials with Schmelzpunkt of 128 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 30 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 30 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property |
---|
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.