Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Platamid® M 1657
Platamid® M 1657
Copolyamide Hot Melt Adhesive / Extrusion Applications
Platamid® M 1657 is a standard thermoplastic co-polyamide hot melt adhesive available in pellet form. This very low melt viscosity, fast re-crystallizing grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments.
Platamid® M 1657 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc).
Platamid® M 1657 has a very good dry cleaning resistance and washing resistance up to 40°C.
This product is available:
PACKAGING
Platamid® M 1657 TA is delivered in 25 kg sealed bags. Platamid®M 1657 FA is delivered in 25 kg sealed bags and 500 kg sealed big bags (GRVS). These grades are ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Diese Materialdaten wurden von Arkema Technical Polymers zur Verfügung gestellt
All categories
Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | dry | ISO 1183 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 107 °C Show Supplier Material materials with Schmelzpunkt of 107 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 200 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 200 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Accessories |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.