Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 25 % Show Supplier Material materials with Bio-based content of 25 % | ||
Dichte | 1.06 g/cm³ Show Supplier Material materials with Dichte of 1.06 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Streckgrenze | 38 MPa Show Supplier Material materials with Streckgrenze of 38 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 102 °C Show Supplier Material materials with Schmelzpunkt of 102 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 26 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 26 cm³/10min | dry | ISO 1133 | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hot Melt Hot Melt Adhesives Automotive Interior - Automotive Interior |