Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1 g/cm³ Show Supplier Material materials with Dichte of 1 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.1 GPa Show Supplier Material materials with Elastizitätsmodul of 1.1 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 13 % Show Supplier Material materials with Elongation at yield of 13 % | cond. | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 18 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 18 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 75 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 75 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | cond. | ISO 527-1/-2 | ||
35 MPa Show Supplier Material materials with Streckgrenze of 35 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 176 °C Show Supplier Material materials with Schmelzpunkt of 176 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 0.4 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 0.4 cm³/10min | dry | ISO 1133 | 275°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Auto - Water Cooling Circuit | |
Processing methods | Injection Molding: |