Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.585 GPa Show Supplier Material materials with Elastizitätsmodul of 0.585 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 26 % Show Supplier Material materials with Elongation at yield of 26 % | dry | ISO 527-1/-2 | ||
Härte, Shore D | 65 [-] Show Supplier Material materials with Härte, Shore D of 65 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 82 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 82 kJ/m² | dry | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry | ISO 179/1eU | ||
Streckgrenze | 28 MPa Show Supplier Material materials with Streckgrenze of 28 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 174 °C Show Supplier Material materials with Schmelzpunkt of 174 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 1.2 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1.2 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines,Tubing and Hoses |