Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.44 GPa Show Supplier Material materials with Elastizitätsmodul of 0.44 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 25 % Show Supplier Material materials with Elongation at yield of 25 % | cond. | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 25 MPa Show Supplier Material materials with Streckgrenze of 25 MPa | cond. | ISO 527-1/-2 | ||
27 MPa Show Supplier Material materials with Streckgrenze of 27 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 173 °C Show Supplier Material materials with Schmelzpunkt of 173 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 14 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 14 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines | |
Processing methods | Injection Molding: |