Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | |
Elastizitätsmodul | 0.332 GPa Show Supplier Material materials with Elastizitätsmodul of 0.332 GPa | cond. | ISO 527-1/-2 | ||
0.34 GPa Show Supplier Material materials with Elastizitätsmodul of 0.34 GPa | dry | ISO 527-1/-2 | |||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 2.4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2.4 kJ/m² | dry | ISO 179/1eA | No Break at 23°C |
-30 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU | ||
Streckgrenze | 44 MPa Show Supplier Material materials with Streckgrenze of 44 MPa | cond. | ISO 527-1/-2 | ||
50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 180 °C Show Supplier Material materials with Schmelzpunkt of 180 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 8 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Brake Tubing,Fuel Management - Fuel Lines |