Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.38 GPa Show Supplier Material materials with Elastizitätsmodul of 0.38 GPa | cond. | ISO 527-1/-2 | ||
0.43 GPa Show Supplier Material materials with Elastizitätsmodul of 0.43 GPa | dry | ISO 527-1/-2 | |||
Elongation at yield | 24 % Show Supplier Material materials with Elongation at yield of 24 % | dry | ISO 527-1/-2 | ||
26 % Show Supplier Material materials with Elongation at yield of 26 % | cond. | ISO 527-1/-2 | |||
Puncture energy | -30 °C | 60 J Show Supplier Material materials with Puncture energy of 60 J | cond. | ISO 6603-2 | |
Puncture force | -30 °C | 5600 N Show Supplier Material materials with Puncture force of 5600 N | cond. | ISO 6603-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00014 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00014 1/K | dry | ISO 11359-1/-2 | |
Schmelzpunkt | 174 °C Show Supplier Material materials with Schmelzpunkt of 174 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 130 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 130 °C | ISO 306 | 50°C/h 50N |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 24 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 24 kV/mm | cond. | IEC 60243-1 |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 |
Surface resistivity | 5e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 5e+11 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+09 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+09 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 16 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 16 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Brake Tubing,Fuel Management - Fuel Lines,Pneumatic Tubing,Tubing and Hoses,Sports Equipment,Antitermite Cables,Performance Wire,Underground Fuel Containment | |
Processing methods | Injection Molding: |