Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.6 % Show Supplier Material materials with Wasserabsorption of 1.6 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | cond. | ISO 527-1/-2 | ||
1.5 GPa Show Supplier Material materials with Elastizitätsmodul of 1.5 GPa | dry | ISO 527-1/-2 | |||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | cond., dry | ISO 527-1/-2 | ||
Puncture energy | -30 °C | 60 J Show Supplier Material materials with Puncture energy of 60 J | cond. | ISO 6603-2 | |
Puncture force | -30 °C | 4800 N Show Supplier Material materials with Puncture force of 4800 N | cond. | ISO 6603-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 31 MPa Show Supplier Material materials with Streckgrenze of 31 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.0001 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0001 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 180 °C Show Supplier Material materials with Schmelzpunkt of 180 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 142 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 142 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB and yellow card available |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | cond. | IEC 60243-1 |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 8 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Pneumatic Tubing,Tubing and Hoses,Footwear - Outsoles,Accessories,Antitermite Cables,Wire and Cables | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |