Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 6 % Show Supplier Material materials with Elongation at yield of 6 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 69 [-] Show Supplier Material materials with Härte, Shore D of 69 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 37 MPa Show Supplier Material materials with Streckgrenze of 37 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 178 °C Show Supplier Material materials with Schmelzpunkt of 178 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 57 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 57 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Schrumpfung | 0.8 % Show Supplier Material materials with Schrumpfung of 0.8 % | dry | ISO 294-4 | |
0.8 % Show Supplier Material materials with Schrumpfung of 0.8 % | dry | ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts,Accessories |