Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.42 GPa Show Supplier Material materials with Elastizitätsmodul of 0.42 GPa | cond. | ISO 527-1/-2 | ||
0.44 GPa Show Supplier Material materials with Elastizitätsmodul of 0.44 GPa | dry | ISO 527-1/-2 | |||
Elongation at yield | 26 % Show Supplier Material materials with Elongation at yield of 26 % | cond., dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 25 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 25 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 38 MPa Show Supplier Material materials with Streckgrenze of 38 MPa | cond. | ISO 527-1/-2 | ||
44 MPa Show Supplier Material materials with Streckgrenze of 44 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00014 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00014 1/K | dry | ISO 11359-1/-2 | |
Schmelzpunkt | 171 °C Show Supplier Material materials with Schmelzpunkt of 171 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 132 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 132 °C | ISO 306 | 50°C/h 50N |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 1MHz | IEC 60250 |
12 [-] Show Supplier Material materials with Dielektrizitätskonstante of 12 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 24 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 24 kV/mm | cond. | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 5e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 5e+11 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.129 [-] Show Supplier Material materials with Verlustfaktor of 0.129 [-] | dry | 1MHz | IEC 60250 |
0.255 [-] Show Supplier Material materials with Verlustfaktor of 0.255 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 1e+09 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+09 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 51 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 51 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Tubing and Hoses | |
Processing methods | Injection Molding: |