Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | Sim. to ISO 62 | |
Sauerstoffindex | 22 % Show Supplier Material materials with Sauerstoffindex of 22 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 1.8 % Show Supplier Material materials with Wasserabsorption of 1.8 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.2 GPa Show Supplier Material materials with Elastizitätsmodul of 1.2 GPa | cond. | ISO 527-1/-2 | ||
1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | dry | ISO 527-1/-2 | |||
Elongation at yield | 7 % Show Supplier Material materials with Elongation at yield of 7 % | cond., dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 42 MPa Show Supplier Material materials with Streckgrenze of 42 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00013 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00013 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 178 °C Show Supplier Material materials with Schmelzpunkt of 178 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 142 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 142 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.5 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: V-2 and yellow card available |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | dry | 1MHz | IEC 60250 |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | cond. | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.029 [-] Show Supplier Material materials with Verlustfaktor of 0.029 [-] | dry | 1MHz | IEC 60250 |
0.0779 [-] Show Supplier Material materials with Verlustfaktor of 0.0779 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 57 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 57 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Schrumpfung | 0.8 % Show Supplier Material materials with Schrumpfung of 0.8 % | dry | ISO 294-4 | |
0.8 % Show Supplier Material materials with Schrumpfung of 0.8 % | dry | ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Monofilaments,Tubing and Hoses | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |