Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.24 g/cm³ Show Supplier Material materials with Dichte of 1.24 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 | |
Wasserabsorption | 1.3 % Show Supplier Material materials with Wasserabsorption of 1.3 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 4 % Show Supplier Material materials with Dehnung of 4 % | cond. | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 6.4 GPa Show Supplier Material materials with Elastizitätsmodul of 6.4 GPa | cond. | ISO 527-1/-2 | |
6.9 GPa Show Supplier Material materials with Elastizitätsmodul of 6.9 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Elongation at yield of 4 % | cond. | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | cond., dry | ISO 179/1eA |
23 °C | 19 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 19 kJ/m² | cond., dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 83 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 83 kJ/m² | dry, cond. | ISO 179/1eU |
23 °C | 77 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 77 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 79 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 79 kJ/m² | dry | ISO 179/1eU | |
Streckgrenze | 115 MPa Show Supplier Material materials with Streckgrenze of 115 MPa | cond. | ISO 527-1/-2 | |
Zugfestigkeit | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | cond. | ISO 527-1/-2 | |
112 MPa Show Supplier Material materials with Zugfestigkeit of 112 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 5e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-05 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 183 °C Show Supplier Material materials with Schmelzpunkt of 183 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Thermal decomposition in air | 227 °C Show Supplier Material materials with Thermal decomposition in air of 227 °C | TGA | 1% wt. loss | ||||
Thermal decomposition in nitrogen | 224 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 224 °C | TGA | 1% wt. loss | ||||
Vicat-Erweichungstemperatur | 165 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 165 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 3.2 mm IEC 60695-11-10: HB and yellow card available |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | dry | 1MHz | IEC 60250 |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 35 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 35 kV/mm | cond., dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.0274 [-] Show Supplier Material materials with Verlustfaktor of 0.0274 [-] | dry | 1MHz | IEC 60250 |
0.0664 [-] Show Supplier Material materials with Verlustfaktor of 0.0664 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 7 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts | |
Certifications | Yellow Card | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding: |