Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.23 g/cm³ Show Supplier Material materials with Dichte of 1.23 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.6 % Show Supplier Material materials with Moisture absorption of 0.6 % | Sim. to ISO 62 | |
Wasserabsorption | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
6 % Show Supplier Material materials with Dehnung of 6 % | cond. | ISO 527-1/-2 | ||
Elastizitätsmodul | 6.5 GPa Show Supplier Material materials with Elastizitätsmodul of 6.5 GPa | cond. | ISO 527-1/-2 | |
6.9 GPa Show Supplier Material materials with Elastizitätsmodul of 6.9 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | cond., dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry | ISO 179/1eA |
-30 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 22 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 22 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 23 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 23 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 93 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 93 kJ/m² | cond. | ISO 179/1eU |
-30 °C | 96 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 96 kJ/m² | dry | ISO 179/1eU | |
23 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 85 kJ/m² | dry | ISO 179/1eU | |
23 °C | 88 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 88 kJ/m² | cond. | ISO 179/1eU | |
Zugfestigkeit | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | cond. | ISO 527-1/-2 | |
122 MPa Show Supplier Material materials with Zugfestigkeit of 122 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 5e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-05 1/K | dry | ISO 11359-1/-2 | |
Schmelzpunkt | 179 °C Show Supplier Material materials with Schmelzpunkt of 179 °C | dry | ISO 11357-1/-3 | 10°C/min |
Thermal decomposition in air | 224 °C Show Supplier Material materials with Thermal decomposition in air of 224 °C | TGA | 1% wt. loss | |
Thermal decomposition in nitrogen | 222 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 222 °C | TGA | 1% wt. loss | |
Vicat-Erweichungstemperatur | 165 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 165 °C | ISO 306 | 50°C/h 50N |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 100Hz | IEC 60250 |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 1MHz | IEC 60250 | |
Durchschlagfestigkeit | 45 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 45 kV/mm | cond. | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.0251 [-] Show Supplier Material materials with Verlustfaktor of 0.0251 [-] | dry | 1MHz | IEC 60250 |
0.0752 [-] Show Supplier Material materials with Verlustfaktor of 0.0752 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 12 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 12 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Sports Equipment | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding: |