Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.06 g/cm³ Show Supplier Material materials with Dichte of 1.06 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastizitätsmodul | 1.7 GPa Show Supplier Material materials with Elastizitätsmodul of 1.7 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry | ISO 179/1eU | |
Streckgrenze | 25 MPa Show Supplier Material materials with Streckgrenze of 25 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 215 °C Show Supplier Material materials with Schmelzpunkt of 215 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Monofilaments |