Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.28 g/cm³ Show Supplier Material materials with Dichte of 1.28 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.8 % Show Supplier Material materials with Moisture absorption of 0.8 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 7.8 GPa Show Supplier Material materials with Elastizitätsmodul of 7.8 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | dry | ISO 179/1eA |
23 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | dry | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | dry | ISO 179/1eU | |
Streckgrenze | 25 MPa Show Supplier Material materials with Streckgrenze of 25 MPa | dry | ISO 527-1/-2 | |
Zugfestigkeit | 137 MPa Show Supplier Material materials with Zugfestigkeit of 137 MPa | dry | ISO 527-1/-2 |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts | |
Fillers | 30% Glass Fiber |