Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.12 - 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.12 - 1.18 g/cm³ | ISO 1183 | relative density |
Mechanisch
Property | Value | Testing Standard |
---|---|---|
Impact energy, coating | 160 J Show Supplier Material materials with Impact energy, coating of 160 J | ASTM D2794 |
Thermisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Schmelzpunkt | 183 - 193 °C Show Supplier Material materials with Schmelzpunkt of 183 - 193 °C | dry | ISO 1218 |
Elektrisch
Property | Value | Testing Standard |
---|---|---|
Durchschlagfestigkeit | 11.8 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 11.8 kV/mm | ASTM D149 |
43.3 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 43.3 kV/mm | ASTM D149 |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Coatings - General Purpose | |
Color | Blue | |
Covering efficiency | 0.35 kg/m² | |
Covering efficiency, thickness | 300 µm |