Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 0.8 % Show Supplier Material materials with Wasserabsorption of 0.8 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 21 % Show Supplier Material materials with Elongation at yield of 21 % | cond. | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | |
Streckgrenze | 42 MPa Show Supplier Material materials with Streckgrenze of 42 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 172 °C Show Supplier Material materials with Schmelzpunkt of 172 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare-Other,IV Bags,Medical Catheters | |
Certifications | Medical | |
Processing methods | Extrusion: |