Allgemein
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 33 % Show Supplier Material materials with Elongation at yield of 33 % | cond. | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 25 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 25 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 100 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 100 kJ/m² | cond. | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 189 °C Show Supplier Material materials with Schmelzpunkt of 189 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Auto - Water Cooling Circuit,Emission Control Systems - SCR Lines and Tanks | |
Processing methods | Injection Molding: |