Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 88 % Show Supplier Material materials with Bio-based content of 88 % | ||
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.6 GPa Show Supplier Material materials with Elastizitätsmodul of 0.6 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 31 % Show Supplier Material materials with Elongation at yield of 31 % | cond. | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 76 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 76 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU | ||
Streckgrenze | 31 MPa Show Supplier Material materials with Streckgrenze of 31 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 184 °C Show Supplier Material materials with Schmelzpunkt of 184 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Air Brake Tubing,Auto - Water Cooling Circuit,Emission Control Systems - Air Conditioning Circuit,Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines | |
Processing methods | Extrusion: |