Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 88 % Show Supplier Material materials with Bio-based content of 88 % | ||
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.6 % Show Supplier Material materials with Wasserabsorption of 1.6 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.35 GPa Show Supplier Material materials with Elastizitätsmodul of 0.35 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 41 % Show Supplier Material materials with Elongation at yield of 41 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 26 MPa Show Supplier Material materials with Streckgrenze of 26 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 182 °C Show Supplier Material materials with Schmelzpunkt of 182 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Air Brake Tubing,Fluid Management - Brakebooster Lines,Fuel Management - Fuel Lines,Fuel Management - In-Tank and Fuel Venting Lines,Performance Wire,Wire and Cables | |
Processing methods | Injection Molding: Extrusion: |