Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 89 % Show Supplier Material materials with Bio-based content of 89 % | ||
Dichte | 1.05 g/cm³ Show Supplier Material materials with Dichte of 1.05 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.6 % Show Supplier Material materials with Wasserabsorption of 1.6 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.335 GPa Show Supplier Material materials with Elastizitätsmodul of 0.335 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 50 % Show Supplier Material materials with Elongation at yield of 50 % | cond. | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 41 MPa Show Supplier Material materials with Streckgrenze of 41 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 181 °C Show Supplier Material materials with Schmelzpunkt of 181 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered dried in sealed packaging (550 kg rigid containers) ready to be processed. Shelf life: Two years from the delivery. For any use above this limit, please refer to our technical services. | |
Processing methods | Extrusion: |