Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1 g/cm³ Show Supplier Material materials with Dichte of 1 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | |
Elastizitätsmodul | 0.19 GPa Show Supplier Material materials with Elastizitätsmodul of 0.19 GPa | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 49 [-] Show Supplier Material materials with Härte, Shore D of 49 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 40 MPa Show Supplier Material materials with Streckgrenze of 40 MPa | cond. | ISO 527-1/-2 | ||
Zugfestigkeit | 36 MPa Show Supplier Material materials with Zugfestigkeit of 36 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 182 °C Show Supplier Material materials with Schmelzpunkt of 182 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore Flexible Pipes |