Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 100 % Show Supplier Material materials with Bio-based content of 100 % | ||
Dichte | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.9 % Show Supplier Material materials with Wasserabsorption of 1.9 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.2 GPa Show Supplier Material materials with Elastizitätsmodul of 1.2 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 71 [-] Show Supplier Material materials with Härte, Shore D of 71 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 36 MPa Show Supplier Material materials with Streckgrenze of 36 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 186 °C Show Supplier Material materials with Schmelzpunkt of 186 °C | dry | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | cond. | IEC 60243-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6 cm³/10min | dry | ISO 1133 | 235°C/10kg |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry - Injection Molding,Packaging / Film,Pneumatic Tubing,Tubing and Hoses | |
Certifications | Food Contact | |
Processing methods | Injection Molding: Extrusion: |