Allgemein
Property | Value |
---|
Mechanisch
Property | Value | Testing Standard |
---|---|---|
Impact energy, coating | 160 J Show Supplier Material materials with Impact energy, coating of 160 J | ASTM D2794 |
Thermisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Schmelzpunkt | 183 - 193 °C Show Supplier Material materials with Schmelzpunkt of 183 - 193 °C | dry | ISO 1218 |
Elektrisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Durchschlagfestigkeit | 200 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 200 kV/mm | ASTM D149 | thickness = 150mm |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Coatings - Automotive & Transportation,Powder Coatings - General Purpose,Powder Coatings - Wire Goods | |
Color | Black | |
Covering efficiency | 0.14 kg/m² | |
Covering efficiency, thickness | 120 µm |