Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 98 % Show Supplier Material materials with Bio-based content of 98 % | ||
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.9 % Show Supplier Material materials with Wasserabsorption of 1.9 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal |
Elastizitätsmodul | 1.6 GPa Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa | cond. | ISO 527-1/-2 | |
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | cond. | ISO 527-1/-2 | |
Härte, Shore D | 70 [-] Show Supplier Material materials with Härte, Shore D of 70 [-] | dry | ISO 7619-1 | 15 seconds |
Streckgrenze | 41 MPa Show Supplier Material materials with Streckgrenze of 41 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-05 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 189 °C Show Supplier Material materials with Schmelzpunkt of 189 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Vicat-Erweichungstemperatur | 162 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 162 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: V-2 and yellow card available |
Elektrisch
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Dielektrizitätskonstante | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | dry | 1MHz | IEC 60250 |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | 100Hz | IEC 60250 | |
Durchschlagfestigkeit | 55 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 55 kV/mm | cond. | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | cond. | IEC 60093 | |
Verlustfaktor | 0.0212 [-] Show Supplier Material materials with Verlustfaktor of 0.0212 [-] | dry | 1MHz | IEC 60250 |
0.0545 [-] Show Supplier Material materials with Verlustfaktor of 0.0545 [-] | dry | 100Hz | IEC 60250 | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | cond. | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 36 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 36 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Monofilaments,Accessories | |
Certifications | Yellow Card | |
Fillers | Mineral Powder | |
Processing methods | Injection Molding: |