Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 100 % Show Supplier Material materials with Bio-based content of 100 % | ||
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 1.9 % Show Supplier Material materials with Wasserabsorption of 1.9 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.3 GPa Show Supplier Material materials with Elastizitätsmodul of 1.3 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 68 [-] Show Supplier Material materials with Härte, Shore D of 68 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 41 MPa Show Supplier Material materials with Streckgrenze of 41 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 189 °C Show Supplier Material materials with Schmelzpunkt of 189 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed. Shelf life: Two years from the delivery. For any use above this limit, please refer to our technical services. | |
Processing methods | Extrusion: |