Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 97 % Show Supplier Material materials with Bio-based content of 97 % | ||
Dichte | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | dry | ISO 1183 |
Sauerstoffindex | 22 % Show Supplier Material materials with Sauerstoffindex of 22 % | dry | ISO 4589-1/-2 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 26 % Show Supplier Material materials with Dehnung of 26 % | cond. | ISO 527-1/-2 | ||
Elastizitätsmodul | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 73 [-] Show Supplier Material materials with Härte, Shore D of 73 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 88 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 88 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 93 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 93 kJ/m² | cond. | ISO 179/1eU | ||
Streckgrenze | 66 MPa Show Supplier Material materials with Streckgrenze of 66 MPa | cond. | ISO 527-1/-2 | ||
76 MPa Show Supplier Material materials with Streckgrenze of 76 MPa | dry | ISO 527-1/-2 | |||
Zugfestigkeit | 56 MPa Show Supplier Material materials with Zugfestigkeit of 56 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 6e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6e-05 1/K | dry | ISO 11359-1/-2 | ||||
Schmelzpunkt | 189 °C Show Supplier Material materials with Schmelzpunkt of 189 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 18 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 18 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Chemical Process Industry - Injection Molding,Footwear - Outsoles,Sports Equipment | |
Fillers | 8% Glass Fiber | |
Processing methods | Injection Molding: |