Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1 g/cm³ Show Supplier Material materials with Dichte of 1 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.7 GPa Show Supplier Material materials with Elastizitätsmodul of 1.7 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 7 % Show Supplier Material materials with Elongation at yield of 7 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 76 [-] Show Supplier Material materials with Härte, Shore D of 76 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 74 MPa Show Supplier Material materials with Streckgrenze of 74 MPa | cond. | ISO 527-1/-2 | ||
76 MPa Show Supplier Material materials with Streckgrenze of 76 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | 101 °C Show Supplier Material materials with Glasübergangstemperatur of 101 °C | dry | ISO 11357-1/-2 | 10°C/min |
Optisch
Property | Value | Testing Standard |
---|---|---|
Lichttransmission | 92 [-] Show Supplier Material materials with Lichttransmission of 92 [-] | ISO 13468-1/2 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 8 cm³/10min | dry | ISO 1133 | 275°C/2.16kg |
Schrumpfung | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | dry | ISO 294-4 | |
0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | dry | ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Eyewear Frames |