Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.05 g/cm³ Show Supplier Material materials with Dichte of 1.05 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | Sim. to ISO 62 | |
Sauerstoffindex | 26 % Show Supplier Material materials with Sauerstoffindex of 26 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 3.8 % Show Supplier Material materials with Wasserabsorption of 3.8 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 2.0 GPa Show Supplier Material materials with Elastizitätsmodul of 2.0 GPa | cond. | ISO 527-1/-2 | ||
2.1 GPa Show Supplier Material materials with Elastizitätsmodul of 2.1 GPa | dry | ISO 527-1/-2 | |||
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 | ||
9 % Show Supplier Material materials with Elongation at yield of 9 % | cond. | ISO 527-1/-2 | |||
Härte, Shore D | 79 [-] Show Supplier Material materials with Härte, Shore D of 79 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at -30°C | dry and cond. | ISO 179/1eU | ||
Streckgrenze | 74 MPa Show Supplier Material materials with Streckgrenze of 74 MPa | cond. | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glasübergangstemperatur | 168 °C Show Supplier Material materials with Glasübergangstemperatur of 168 °C | dry | ISO 11357-1/-2 | 10°C/min | |||
Koeffizient der thermischen Ausdehnung | 7e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-05 1/K | dry | ISO 11359-1/-2 | ||||
Vicat-Erweichungstemperatur | 160 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 160 °C | ISO 306 | 50°C/h 50N | ||||
Entflammbarkeit | At thickness 1.6 mm IEC 60695-11-10: V-2 and yellow card available |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 50 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 50 kV/mm | cond. | IEC 60243-1 |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | cond. | IEC 60112 |
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | cond. | IEC 60093 |
Optisch
Property | Value | Testing Standard |
---|---|---|
Lichttransmission | 91 [-] Show Supplier Material materials with Lichttransmission of 91 [-] | ISO 13468-1/2 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 2 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 2 cm³/10min | dry | ISO 1133 | 275°C/2.16kg |
Schrumpfung | 0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | dry | ISO 294-4 | |
0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | dry | ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Home Appliance Tubing and Components | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: Film Extrusion: |