Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 45 % Show Supplier Material materials with Bio-based content of 45 % | ||
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | Sim. to ISO 62 | |
Wasserabsorption | 4 % Show Supplier Material materials with Wasserabsorption of 4 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.7 GPa Show Supplier Material materials with Elastizitätsmodul of 1.7 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 78 [-] Show Supplier Material materials with Härte, Shore D of 78 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 7.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7.5 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | 150 °C Show Supplier Material materials with Glasübergangstemperatur of 150 °C | dry | ISO 11357-1/-2 | 10°C/min |
Optisch
Property | Value | Testing Standard |
---|---|---|
Lichttransmission | 92 [-] Show Supplier Material materials with Lichttransmission of 92 [-] | ISO 13468-1/2 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Breathing Masks,Healthcare-Other | |
Certifications | USP Class VI | |
Processing methods | Injection Molding: |