Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.1 g/cm³ | ISO 1183 | relative density |
Median particles size | 30 μm Show Supplier Material materials with Median particles size of 30 μm | ISO 13320 | |
Non Tap density | 0.44 g/cm³ Show Supplier Material materials with Non Tap density of 0.44 g/cm³ | ISO 1068 | |
Tap density | 0.62 g/cm³ Show Supplier Material materials with Tap density of 0.62 g/cm³ | ISO 1068 | |
Wasserabsorption | 1 % Show Supplier Material materials with Wasserabsorption of 1 % | ISO 62-1 | max. | for 24h |
Mechanisch
Property | Value | Testing Standard | |
---|---|---|---|
Hardness, Persoz | 270 [-] Show Supplier Material materials with Hardness, Persoz of 270 [-] | ISO 1522 | |
Hardness, Pencil test | ECCA T4: B |
Thermisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Schmelzpunkt | 183 - 188 °C Show Supplier Material materials with Schmelzpunkt of 183 - 188 °C | dry | ISO 1218 |
Elektrisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Durchschlagfestigkeit | 10 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 10 kV/mm | ASTM D149 | thickness = 100mm |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Coatings - General Purpose | |
Color | Grey | |
Covering efficiency | 0.2 kg/m² | |
Covering efficiency, thickness | 100 µm |