Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 45 % Show Supplier Material materials with Bio-based content of 45 % | ||
Dichte | 1.05 g/cm³ Show Supplier Material materials with Dichte of 1.05 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 1.0 GPa Show Supplier Material materials with Elastizitätsmodul of 1.0 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 66 [-] Show Supplier Material materials with Härte, Shore D of 66 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 84 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 84 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU | ||
Streckgrenze | 64 MPa Show Supplier Material materials with Streckgrenze of 64 MPa | cond. | ISO 527-1/-2 |
Thermisch
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 1.9 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 1.9 cm³/10min | dry | ISO 1133 | 300°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Auto - Water Cooling Circuit,Emission Control Systems - Air Conditioning Circuit,Emission Control Systems - Vacuum and Blow by Lines,Fluid Management - Brakebooster Lines,Fluid Management - Transmission oil Cooling Circuit | |
Processing methods | Profile Extrusion: |