Allgemein
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 2.4 GPa Show Supplier Material materials with Elastizitätsmodul of 2.4 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 81 [-] Show Supplier Material materials with Härte, Shore D of 81 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 59 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 59 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 38 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 38 kJ/m² | cond. | ISO 179/1eU |
Thermisch
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 10 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 10 cm³/10min | dry | ISO 1133 | 255°C/2.16kg |
Schrumpfung | 1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | dry | ISO 294-4 | Transverse |
1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | dry | ISO 294-4 |
Technological properties
Property | ||
---|---|---|
Application areas | Monofilaments | |
Processing methods | Injection Molding: Profile Extrusion: |