Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 67 % Show Supplier Material materials with Bio-based content of 67 % | ||
Dichte | 1.3 g/cm³ Show Supplier Material materials with Dichte of 1.3 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.22 % Show Supplier Material materials with Moisture absorption of 0.22 % | Sim. to ISO 62 | |
Wasserabsorption | 1.13 % Show Supplier Material materials with Wasserabsorption of 1.13 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 4 % Show Supplier Material materials with Dehnung of 4 % | cond. | ISO 527-1/-2 | ||
Elastizitätsmodul | 8.5 GPa Show Supplier Material materials with Elastizitätsmodul of 8.5 GPa | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 83 [-] Show Supplier Material materials with Härte, Shore D of 83 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 46 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 46 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 51 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 51 kJ/m² | cond. | ISO 179/1eU | ||
Streckgrenze | 45 MPa Show Supplier Material materials with Streckgrenze of 45 MPa | dry | ISO 527-1/-2 | ||
Zugfestigkeit | 130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | cond. | ISO 527-1/-2 |
Thermisch
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 15 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 15 cm³/10min | dry | ISO 1133 | 300°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Auto - Water Cooling Circuit | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding: |