Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 59 % Show Supplier Material materials with Bio-based content of 59 % | ||
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.45 % Show Supplier Material materials with Moisture absorption of 0.45 % | Sim. to ISO 62 | |
Wasserabsorption | 1.1 % Show Supplier Material materials with Wasserabsorption of 1.1 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 0.21 GPa Show Supplier Material materials with Elastizitätsmodul of 0.21 GPa | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 53 [-] Show Supplier Material materials with Härte, Shore D of 53 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | cond. | ISO 179/1eA | No Break at 23°C |
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 188 °C Show Supplier Material materials with Schmelzpunkt of 188 °C | dry | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1.9e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1.9e+13 Ω·cm | dry | IEC 60093 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 4 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 4 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Main applications: Packaging: This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed. Shelf life: Two years from the delivery. For any use above this limit, please refer to our technical services. | |
Processing methods | Extrusion: |