Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 60 % Show Supplier Material materials with Bio-based content of 60 % | ||
Dichte | 1.31 g/cm³ Show Supplier Material materials with Dichte of 1.31 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastizitätsmodul | 8.3 GPa Show Supplier Material materials with Elastizitätsmodul of 8.3 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 89 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 89 kJ/m² | dry | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | dry | ISO 179/1eU |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |