Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.11 g/cm³ Show Supplier Material materials with Dichte of 1.11 g/cm³ | ISO 1183 | relative density |
Fluidized density | 0.5 [-] Show Supplier Material materials with Fluidized density of 0.5 [-] | ||
Median particles size | 100 - 130 μm Show Supplier Material materials with Median particles size of 100 - 130 μm | ISO 13320 | |
Non Tap density | 0.57 g/cm³ Show Supplier Material materials with Non Tap density of 0.57 g/cm³ | ISO 1068 | |
Tap density | 0.69 g/cm³ Show Supplier Material materials with Tap density of 0.69 g/cm³ | ISO 1068 | |
Wasserabsorption | 1 % Show Supplier Material materials with Wasserabsorption of 1 % | ISO 62-1 | max. | for 24h |
Mechanisch
Thermisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Schmelzpunkt | 183 - 188 °C Show Supplier Material materials with Schmelzpunkt of 183 - 188 °C | dry | ISO 1218 |
Elektrisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | ASTM D149 | thickness = 350-450mm |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Coatings - Exterior Applications,Powder Coatings - Fluids Transportation,Powder Coatings - General Purpose,Powder Coatings - Mining,Powder Coatings - Wire Goods | |
Color | Grey | |
Covering efficiency | 0.35 kg/m² | |
Covering efficiency, thickness | 300 µm |