Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.09 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | Sim. to ISO 62 | |
Wasserabsorption | 2.9 % Show Supplier Material materials with Wasserabsorption of 2.9 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.515 GPa Show Supplier Material materials with Elastizitätsmodul of 0.515 GPa | cond. | ISO 527-1/-2 | ||
0.685 GPa Show Supplier Material materials with Elastizitätsmodul of 0.685 GPa | dry | ISO 527-1/-2 | |||
Elongation at yield | 31 % Show Supplier Material materials with Elongation at yield of 31 % | cond. | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6.5 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 95 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 95 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 217 °C Show Supplier Material materials with Schmelzpunkt of 217 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 3.7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 3.7 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - In-Tank and Fuel Venting Lines | |
Processing methods | Extrusion: |